High Silicon Cast Iron Tubular Anode
Feature:

YUXI's tubular high silicon cast iron anodes are manufactured using a centrifugal chill cast method. No other method consistently produces tubular anodes with a superior metallic structure than this proven route. We manufacture anodes both in UK and China with a combined production capacity of 3000 tons per year.


CHEMICAL COMPOSITION

We developed rigid controls for the chill casting process in accordance with the highest standards — meeting X-Ray Level 1 as per ASTM E186/E446, chemistry to either ASTM A518-99 Gr 1 or 3. ASTM A518 Grade 3 chemistry is particularly suited for more severe environments(such as brackish water or saltwater), where the level of chromium is elevated to enhance anode performance.


◉ ASTM A518/A518M Grade 1 (Si-Fe)

Element

Content (%)

Silicon (Si)
14.20 ~ 14.75
Chromium (Cr)
0.500 max.
Manganese (Mn)
1.500 max.
Copper (Cu)
0.500 max.
Molybdenum (Mo)
0.500 max.
Carbon (C)
0.650 ~ 1.100
Phosphorus (P)
-
Sulphur (S)
-
Iron (Fe)
Remainder


◉ ASTM A518 / A518M Grade 3 (Si-Fe-Cr)

Element

Content (%)

Silicon (Si)
14.20 ~ 14.75
Chromium (Cr)
3.250 ~ 5.000
Manganese (Mn)
1.500 max.
Copper (Cu)
0.500 max.
Molybdenum (Mo)
0.200 max.
Carbon (C)
0.700 ~ 1.100
Phosphorus (P)
-
Sulphur (S)
-
Iron (Fe)
Remainder


◉ BS 1591 1975

Element

Content (%)

Silicon (Si)
14.25 ~ 15.25
Chromium (Cr)
0.500 max.
Manganese (Mn)
0.500 max.
Copper (Cu)
-
Molybdenum (Mo)
-
Carbon (C)
1.400 max.
Phosphorus (P)
0.250 max.
Sulphur (S)
0.100 max.
Iron (Fe)
Remainder


ELECTROCHEMICAL PROPERTIES

Due to its high content of silicon, the anode surface is readily and continually oxidized with a thin film of hydrated silicon oxides, which protects the anode from metal pitting. Our high silicon cast iron anodes exhibit extraordinary corrosion resistance and low consumption rate in low-pH environment.


◉ Soil

Technical Measurement

Performance

Current Density (A/m²) 2 ~ 5
Consumption Rate (kg/A.y)
0.1 ~ 0.5


◉ Coke Breeze

Technical Measurement

Performance

Current Density (A/m²) 5 ~ 10
Consumption Rate (kg/A.y)
0.05 ~ 0.3


PRACTICAL APPLICATION

Our high silicon cast iron tubular anodes are widely used to protect buried and submerged structures from corrosion, such as pipelines, offshore oil drilling platforms, etc. Normally, quick installation of 200 pieces anodes via specialized connector can be